Author Gabrian The Extrusion Die is Prepared and Moved to the Extrusion Press. First, a round-shaped die is An Aluminum Billet is Preheated Before Extrusion. Next, a solid, cylindrical block of aluminum The Billet is Transferred to the Extrusion Press. Once the billet has been preheated, it is The Ram Pushes the Billet Material into the Container. Now, the malleable billet is loaded into the The Extruded Material Emerges Through the Die. As the alloy material fills the container, it is now Extrusions are Guided Along the Runout Table and Quenched. After emerging, the extrusion is Extrusions are Sheared to Table Length. Once an extrusion reaches its full table length, it is Extrusions are Cooled to Room Temperature. After shearing, table-length extrusions are Extrusions are Moved to the Stretcher and Stretched into Alignment. Some natural twisting has Extrusions are Moved to the Finish Saw and Cut to Length. With the table-length extrusions now